Typical Total Thickness |
N/A 3.0 mil |
Typical Water Vapour Transmission Rate |
N/A 0.4560 g/100 in²/24hrs |
Test Method (Water Vapour Transmission Rate) |
N/A ASTM F-1249-90 |
Typical Transmission Rate |
N/A 3.5 to 4.5 cc/100 in²/24hrs |
Typical Tensile Strength Machine Direction (MD) |
N/A 4800 psi |
Typical Tensile Strength Transverse Direction (TD) |
N/A 3800 psi |
Test Method (Tensile Strength) |
N/A ASTM D882-91; A |
Typical Tear Strength Machine Direction (MD) |
N/A 2.1 lb |
Typical Tear Strength Transverse Direction (TD) |
N/A 2.8 lb |
Test Method (Tear) |
N/A ASTM D1004-94 (MD) NOTCHED (CD) |
Typical Elongation Machine Direction (MD) |
N/A 450 % |
Typical Elongation Transverse Direction (TD) |
N/A 550 % |
Test Method (Elongation) |
N/A ASTM D882-91: A |
Typical Puncture Strength |
N/A 20.5 lb |
Test Method (Puncture Strength) |
N/A FTMS 101-C; 2065.1 |
Typical Light Transmission |
N/A >90 % |
Test Method (Light Transmission) |
N/A ASTM D1003-92 |
Typical Heat Seal Strength |
N/A 22 lb/in width |
Test Method (Heat Seal Strength) |
N/A ASTM D-1876-93 VERTROD |